Arcam launches a nickel base superalloy process for additive manufacturing with Arcam's EBM systems

09/06/2014

Press releaseIssued by Colibrium Additive (was GE Additive - Arcam EBM).

Arcam today launches a process for Inconel 718® as a qualified material for use in Arcam's EBM systems. The Inconel process is initially available for the Arcam A2X platform. The machine material parameters and mechanical testing was done in collaboration with the U.S. Department of Energy's Manufacturing Demonstration Facility at Oak Ridge National Laboratory. Parts made in the new process are exhibited at the Rapid conference in Detroit, MI, June 10-12.

“With the introduction of the Inconel 718 our customers in the aerospace industry can now further expand the range of components that they produce in their EBM machines”, says Magnus René, CEO of Arcam.

The material properties comply with chemical requirements of UNS N07718 and properties of ASTM F3055-14 specification.

The industry ledger — an Analytics feature — collects the dated facts behind stories like this one, filterable by theme, company, program, country and date. See a worked example →

In this release

Sectors covered
Your news here

Submit your press releases

Send releases and photographs to news@news.airframer.com — the pick of them reach Bulletin readers every Thursday.

Every Thursday

The Airframer Bulletin

The week’s aerospace manufacturing news, reported by our editors and delivered free to your inbox. Sign up ›

Go deeper

Who supplies whom?

Subscribers see the confirmed supply chain behind every story — complete supplier lists for each aircraft program, sector and company. See the plans ›

Spotted something wrong or out of date on this page? Tell us

Corrections go straight to the editorial team that maintains this directory.