Velo3D qualifies new superalloy for use in its Sapphire family of printers

06/01/2022

Press releaseIssued by Velo3D.

Velo3D, Inc., a leading metal additive manufacturing technology company for mission-critical parts, has qualified the nickel-based superalloy powder Amperprint 0233 Haynes 282 for use in its Sapphire family of printers. The powder was produced by Hoganas AB—a world leader in metal powder production—under license from Haynes International, Inc., and is designed for high creep strength, thermal stability, weldability, and fabricability not commonly found in other alloys. The material is ideal for high-temperature structural applications like energy generation, gas turbines, and space launch vehicles to build parts like heat exchangers, combustors, nozzles, combustion liners, rocket engines, and shrouded impellers.

The first Sapphire printer utilising the Amperprint 0233 Haynes 282 powder will be operated by Duncan Machine Products (DMP), a contract manufacturer based in Duncan, Oklahoma. The system will be the seventh in DMP's fleet of Velo3D Sapphire printers.

"Our goal at Velo3D is to enable engineers to build the parts they want without compromising on the design or quality," said Benny Buller, Velo3D CEO and Founder. "Qualifying new powdered metals, like Amperprint 0233 Haynes 282, for use in our end-to-end solution, further expands what's possible with our additive manufacturing technology. Our partners at Hoganas provide materials of the highest quality, and I look forward to seeing what our customers build using this amazing alloy."

Powdered nickel-based superalloys, like Amperprint 0233 Haynes 282, are often used to print parts for use in high-temperature applications due to the alloy's resistance to cracking and its ability to operate at near-melting-point temperatures. This tolerance allows parts printed with the alloy to be used in vacuum, plasma, and other demanding applications. Its high weldability makes the powder ideal for parts in larger systems because of its ability to be welded to other components.

Hoganas specialises in creating powders for additive manufacturing, delivering products with consistent spherical shape, tight control on chemistry, and enhanced flowability. The powders are made using the purest materials with very precise compositions of trace elements that give the metals their unique properties.

"It's inspiring to see what engineers have been able to build using metal powders from Hoganas and Velo3D's support-free additive manufacturing process," said Jerome Stanley, Hoganas Director of Global Sales, Customisation Technologies. "The first parts printed using our Amperprint 0233 Haynes 282 powder are impressive, and I believe customers are only scratching the surface of what is possible with this superalloy. The powder, combined with Velo3D's end-to-end solution metal AM solution, is an extremely effective combination for consolidating parts into monolithic structures to eliminate coefficient of thermal expansion in large, high-performance systems."

Velo3D is one of the first additive manufacturing technology companies to offer Amperprint 0233 Haynes 282 powder to its customers. Many of Velo3D's customers use its end-to-end solution to produce parts for use in aviation, energy, oil and gas, space, and other high-performance applications, making the powder a good fit for Velo3D's portfolio. In addition to Amperprint 0233 Haynes 282 powder, metal powders qualified to be printed with Velo3D's technology include Hastelloy X, Inconel 718, aluminum F357, Ti 6Al-4V Grade 5, and several additional materials.

The industry ledger — an Analytics feature — collects the dated facts behind stories like this one, filterable by theme, company, program, country and date. See a worked example →

In this release

Sectors covered
Companies covered
Your news here

Submit your press releases

Send releases and photographs to news@news.airframer.com — the pick of them reach Bulletin readers every Thursday.

Every Thursday

The Airframer Bulletin

The week’s aerospace manufacturing news, reported by our editors and delivered free to your inbox. Sign up ›

Go deeper

Who supplies whom?

Subscribers see the confirmed supply chain behind every story — complete supplier lists for each aircraft program, sector and company. See the plans ›

Spotted something wrong or out of date on this page? Tell us

Corrections go straight to the editorial team that maintains this directory.